316S33(1.4436)线性膨胀系数

2022-12-13 21:20 作者:上海珑技  | 我要投稿

316S33(1.4436)板,棒,管,钢带,线材,锻件,锻管,锻板,锻棒,圆棒,板材,薄板,无缝管,焊管,圆钢,丝材

牌号

316S33

Bs 970-3-1991

对应标准

机械及相关工程用钢的规格第3部分:—般工程用优质钢棒

Specification for wrought steel for machanical and allied engineering purposes part 3.:bright bars for general engineering purposes

归类

奥氏体不锈钢

性能强度耐腐蚀低温韧性冲击韧性锻压性

标签

奥氏体不锈钢

316S33(1.4436)不锈钢是在316的基础上加入了氢,但碳含量处于其的上限,多用于热强性能较不含钼钢要求

更高的耐热用途,具有良好的加工性能、焊接性能,高温抗氧化性能。

316S33 (1.4436) stainless steel is added with hydrogen on the basis of 316, but the carbon content is at its upper limit, which is mostly used for the requirements of thermal strength properties rather than molybdenum containing steel

Higher heat resistance, good processing performance, welding performance, high temperature oxidation resistance.

316S33 化学元素成分含量(%)

316S33 机械性能

316S33不锈钢应用领域:主要用于耐点蚀材料上

使用。可用耐热要求的锅炉过热器,热交换器,催化器,冷凝器等的钢管和管件。

Application field of 316S33 stainless steel: mainly used for pitting resistant materials

use. Steel pipes and fittings for boiler superheater, heat exchanger, catalyst, condenser, etc. with heat resistance requirements can be used.

物理性能

抗拉强度,R m : 500 - 700 MPa

屈服点,R p0,2 : >200 MPa

伸长率,A:>40%

弹性模量,E:200 GPa

硬度,HB:<215

电阻率,Ω:0,75 mkOhm * m

热容量,c p : 500 J * kg -1 * K -1

导热系数,λ:15 W * m -1 * K -1

线性膨胀系数,α:16,0 * 10 -6 K -1

工艺和温度:

钢在 1020 - 1120 ℃ 水或空气冷却的超淬火

1.4435/1.4436钢在1200-900℃的轧制和锻造

1.4432 钢在 1150 - 850 °C 下的轧制和锻造

physical property

Tensile strength, Rm: 500 - 700 MPa

Yield point, R p0,2:>200 MPa

Elongation, A:>40%

Elastic modulus, E: 200 GPa

Hardness, HB:<215

Resistivity, Ω: 0,75 mkOhm * m

Heat capacity, c p: 500 J * kg - 1 * K - 1

thermal conductivity, λ: 15 W * m -1 * K -1

Coefficient of linear expansion, α: 16,0 * 10 -6 K -1

Process and temperature:

Super Quenching of Steel Cooled with Water or Air at 1020 - 1120 ℃

Rolling and forging of 1.4435/1.4436 steel at 1200-900 ℃

Rolling and forging of 1.4432 steel at 1150 - 850 ° 